© 2018 R3 Tech. All rights reserved.

OUR APPLICATION

PANEL BACKSHEETS

FACT

01/

Insufficient Testing Standards

Despite PET, PVDF, and PA-based backsheets passing IEC and solar panel manufacturer requirements, current testing standards are insufficient to ensure long-lasting durability and reliability of solar materials

02/

Premature Defective Panels

PA, PET, AAA Backsheets have shown cracking, yellowing and delamination in just 4 to 5 years

03/

Global key concern

North America, Europe, India, South Africa and China are among the main geographical areas

Root cause:

Ultraviolet Light

Extreme Temperatures

Moisture

Thermal Cycling

SOLUTION

R3 Tech uses a state of the art laminating material to fix the backsheets that can then extend its lifespan for another 10 more years. This innovation is the answer to the root cause of the problem.

You have the option of repairing it yourself with our guided process or we can repair it on-site for you.*

* Based on utility scale volume

WEARABILITY
UV RADIATION
STRICT QA

JUNCTION BOX

FACT

Defective Junction Boxes

Within a period of 5 years after the initial installation, Junction Boxes’ failure is contributed by burnt bypass diode, burnt JB or low power. 85% of failure caused by system install sector and barely from module of JB suppliers.

Burnt Junction Box

SOLUTION

R3 TECH teams up with global PV experts to replace defective Junction Boxes wherever they are. Once the enquiry form is duly completed, we will give our best quote.

Don’t wait and contact us now!